Follow us on:

Tikkurila Temafloor PU UV | Floor Paint

Tikkurila Temafloor PU UV

473
TIK4732

A solvent-free polyurethane paint, that has excellent UV-resistance and withstands mechanical and chemical stresses. It`s also a high-solids, flexible and weather resistant two-component polyurethane coating.

  • Excellent resistance to UV.
  • Silent, does not shrink or crack.
  • Withstands mechanical and chemical stress.
  • Self-levelling, to be applied with serrated or steel trowel.
  • Intended to be used as a UV-resistant topcoat on Temafloor PU floors in parking decks and other areas exposed to direct sunlight.

Professional use only - from the 24th August 2023, adequate training is required before industrial or professional use of this product.

Should you require training, visit - https://www.safeusediisocyanates.eu/

Colour
Pick a Colour
  • Current colour: TVT 0229
Close colour picker
  • RAL3001 - Signal Red
  • RAL7032 - Pebble Grey
  • RAL7040 - Window Grey
  • TVT 0229
Size
Finish
£452.64(incl. VAT)
£377.20(ex. VAT)
Quantity
Please choose your colour
Please Contact our Technical Team on 0113 245 5450 (ext. 2) to Order this Product

No queries yet, leave the first!
Description

Professional use only - from the 24th August 2023, adequate training is required before industrial or professional use of this product.

Should you require training, visit - https://www.safeusediisocyanates.eu/

Tikkurila Temafloor PU UV is a solvent-free polyurethane paint, that has excellent UV-resistance and withstands mechanical and chemical stresses. It's also a high-solids, flexible and weather resistant two-component polyurethane coating.

Temafloor PU-UV is a self-leveling paint and creates seamless smooth surface. The coating is mostly used for e.g. parking decks, footpaths and other areas exposed to abrasion and direct sunlight.



Quick Links - Click To Jump To Section:




Features & Benefits


  • Excellent resistance to UV
  • Silent, does not shrink or crack
  • Withstands mechanical and chemical stress
  • Self-levelling, to be applied with serrated or steel trowel
  • Intended to be used as a UV-resistant topcoat on Temafloor PU floors in parking decks and other areas exposed to direct sunlight



Technical Data


Technical Data
Tikkurila Temafloor PU UV
Volume Solids: approx. 90%
SG: 1.4 kg / litre (mixture)
Viscosity: n/a
Density: 1.6 to 1.7 g/cm³ - Hardener: 1.07 g/cm³
Storage Conditions: Store away from direct sunlight in a dry, cool and well-ventilated area, away from incompatible materials (see Section 10). Keep container tightly closed. Containers that have been opened must be carefully resealed and kept upright to prevent leakage. Do not store in unlabeled containers. Recommended storage temperature is +5°C ...+25°C
Shelf Life: None
Pot Life: 40 minutes on substrate, abt. 20 minutes in the mixing container.
Flash Point: >100˚C - Hardener: Closed cup: 35°C
Coverage (for a flat substrate): Practical coverage depends on the porosity and evenness of the substrate and on the application method.



Drying Times At 23°C
Dust Dry: After 6 hours
Light Trucking: After 24 hours
Fully Cured: After 7 days





Surface Preparation


New Concrete

  • Remove laitance by power grinding vacuum grit blasting or hydrochloric acid etching.
  • Choose the method best suited for the premises.
  • After grinding remove dust carefully with a vacuum cleaner.
  • Hydrochloric acid etching is carried out with diluted hydrochloric acid (1 part concentrated hydrochloric acid, 4 parts water).
  • Rinse with plenty of water.
  • Dry the surface.

Old Concrete

  • Remove all grease, oil, chemicals and other impurities by Maalipesu detergent.
  • Remove old peeling paint layer by grinding.
  • Choose the method best suited for the premises.
  • Clean out pot-holes removing all loose friable material.
  • Open cracks with e.g. an abrasive tool.
  • Remove loose material and dust.

If cementitious screed is used, check compatibility with the levelling screed manufacturer.



Application Conditions


  • The relative humidity of the concrete should not exceed 97%.
  • The temperature of the ambient air, surface or coating should not fall below +15ºC during application or drying.
  • Relative humidity of air should not exceed 70%



Mixing Components


Mixing Ratio
Base: 2 parts by volume Temafloor PU UV
Hardener: 1 part by volume 008 4011



  • First stir base and hardener separately.
  • Mix the correct proportions of base and hardener thoroughly (approx. 2 minutes to get homogenous mixture) by using a low speed industrial hand drill with a paddle.
  • Insufficient mixing or incorrect mixing ratio will result in uneven drying of the surface, weaken the properties of the coating and risk the success of the application.



Thickness
Film thickness 0.3mm coverage approx: 2.7 m²/litre
Film thickness 1.0mm coverage approx: 0.9 m²/litre



Application


Priming:

  • Prime using Temafloor 400 epoxy varnish thinned 30–50% with Thinner 1029 or Fontefloor EP Primer epoxy varnish thinned about 20-50% with water.
  • Pour the primer onto the floor and apply as much as is needed to impregnate the concrete surface.
  • If necessary, repeat priming to get a non-porous surface.
  • A porous priming coat will result in holes and air bubbles in the finished coating.
  • Subsequent treatment can be carried out after 2 hours using "wet-on-wet" technique.
  • Asphalt floors should be primed by applying unthinned Temafloor PU with a suitable steel or rubber trowel.
  • Scatter sand of grain size Ø 0,1–0,6 mm on the fresh primer coat to ensure the screed adhesion and prohibit gliding of the screed.
  • Remove loose sand with vacuum cleaner before coating with Temafloor PU UV.

Patching:

  • Patch pot-holes and cracks with a mixture of unthinned Temafloor 400 epoxy varnish and dry, clean sand.
  • Mixing ratio e.g. 1 part by volume of varnish mixture and 1–2 parts by volume of sand of grain size 0.1–0.6 mm.
  • Sand the patched areas before overcoating, if necessary.
  • Note! Concrete surface should always be primed before patching.

Topcoating:

  • Overcoating may be carried out not earlier than 24 hours after coating with Temafloor PU.
  • If the primed surface is not overcoated within 24 hrs, it should be abraded.
  • Pour the mixture onto the floor and apply it with a trowel and level with a roller.
  • Control that the thickness of layer is correct by observing coating consumption and by measuring the film thickness.
  • Recommended layer thickness is 1.0–2.0 mm.
  • Use spiked roller to finish the surface approx. 10–20 min after application. Spiked roller helps removing air bubbles from the coating.



Thinner/Cleaning


Thinner:

  • Do not thin Temafloor PU UV polyurethane coating.

Cleaning of equipment:



VOC


  • VOC 2004/42/EC (cat A/j)500 g/l (2010)
  • Temafloor PU UV: max. VOC < 500 g/l



Health And Safety


Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets.

For industrial and professional use only.

Click to go back to the top of the page

Product Details
4732-766936

Data sheet

Manufacturer
Tikkurila
For Use By
Professional Use
Single, Two or Three Pack
Two-Pack
Parts
Two part pack
Base Type
Polyurethane
Mixing Ratio
Base: 2 parts by volume Temafloor PU UV - Hardener: 1 part by volume 008 4011
Coverage
Practical coverage depends on the porosity and evenness of the substrate and on the application method.
Density
1.6 to 1.7 g/cm³ - Hardener: 1.07 g/cm³
Solids by Volume
approx. 90%
Finish
Gloss
Size
15L
UN Number
Hardener UN1263
Dry to Recoat (at 23°C)
After 24 hours
Touch Dry (at 23°C)
After 6 hours
Fully Cured (at 23°C)
After 7 days
Pot Life
40 minutes on substrate, abt. 20 minutes in the mixing container.
Suitable For Use On
Polyurethane
Suitable For Use On
Epoxy
Suitable For Use On
Zinc
Suitable For Use On
Aluminium
Suitable For Use On
Stainless Steel
Suitable For Use On
Steel
Suitable For Use On
Concrete Floors
Finish
Matt
Components
2K
Product Usage Type
Self Smoothing Screed
Product Range
Temafloor
Colour Family
Grey
Colour Family
Red
Average Application Thickness
0.3-1mm
Product Type
Polyurethane
Attachments
Download


Customer agrees that before placing an Order, Customer has read and understood the most up to date Product Data Sheet for the Product. Where we have access to the Product Data Sheet from the manufacturer, we will either provide a copy on request, or include a link to the Product Data Sheet available on the manufacturer’s website. Customer further agrees that we have no liability for any errors or omissions contained within the Product Data Sheets. For more information, please see our Terms & Conditions of Sale.

Questions

Question about the product

* Required fields
(read)

Be the first to ask a question about this product!

IMPORTANT SHIPPING & DELIVERY INFORMATION

Tikkurila Temafloor PU UV is only available with the shipping and delivery timescales listed below - please do not contact our Customer Support Team with enquiries about alternative or earlier shipping and delivery times.

Saturdays and Sundays, as well as Bank Holidays, are not classed as working days.

Orders placed after the cut-off for this product will not be processed for earliest dispatch until 9am the next working day.

All delivery costs below are excluding VAT


You might also like
Tikkurila Fontefloor EP Primer | Odourless Priming Lacquer For Concrete

Tikkurila Fontefloor EP Primer

2-component water-borne epoxy lacquer that seals the concrete surface and provides adhesion to all Temafloor coatings and screeds, and Fontefloor paints, and can also be used for patching cracks and holes in concrete. Dries in 6 hours for overcoating Also used for priming of damp concrete with relative humidity over 97% prior to Fontefloor...

Price £455.76 (incl. VAT)
Shop now
Trustpilot
In Stock and Available for Delivery
Tikkurila Temafloor 400 | Epoxy Floor Paint

Tikkurila Temafloor 400

2-component solvent-free epoxy varnish. An excellent product for dust binding and priming of new and old concrete floors, especially where solventless and odourless products are needed. The lacquer can be used for patching when filled with sand. Used as a binder for Temafloor 4000 troweling screed and epoxy concrete. Used also as a topcoat...

Price £397.98 (incl. VAT)
Shop now
Trustpilot
In Stock and Available for Delivery
Tikkurila Thinner 1029 | Solvents & Thinners

Tikkurila Thinner 1029

Tikkurila Thinner 1029 is a thinner for ethyl zinc silicate paints and solvent-free epoxy paints.

Price £88.24 (incl. VAT)
Shop now
Trustpilot
In Stock and Available for Delivery
Tikkurila Thinner 1061 | Solvents & Thinners

Tikkurila Thinner 1061

Tikkurila Thinner 1061 is a fast thinner for polyurethane paints.

Price £190.63 (incl. VAT)
Shop now
Trustpilot
In Stock and Available for Delivery